    Finishing off cutting ot rust and patch panels. Pretty much a beginner (welder and car guy).
    How much bondo (depth) is ok to smooth things out. I have panels that are pretty good where the amount of bondo is only enough to cover edge of weld (maybe 1mm) ....... but otehr areas at joints where I didnt do as well and might be 1-8-1/4" off .......

    Not a show car. DD.
     
  2. FAKKY
    Joined: Sep 9, 2016
    Posts: 295

    FAKKY
    Member

  3. FAKKY
    Joined: Sep 9, 2016
    Posts: 295

    FAKKY
    Member

    not mine ^^^ but similar I would think ......
    Where the panel is not in full alignment with the counter of older panels ...... id definitely need a full 1/4" bondo to smooth out the panel transitions ......
     
  4. FAKKY
    Joined: Sep 9, 2016
    Posts: 295

    FAKKY
    Member

    well heres an actual pic of mine .......
    The lip would be 1/8" to smooth between panels .......... but to align with the other panels better might need to build the entire thing to ~ 1/4" etc patchpanel2.jpg
     
  5. This is where reading the TDS of the products you are using comes in handy. The max recommended thickness for regular fillers is usually 1/4". If you are going to be pushing that then you should use a reinforced product underneath and then skim with a regular body filler.
     
  6. FAKKY
    Joined: Sep 9, 2016
    Posts: 295

    FAKKY
    Member

    good point - didnt even think of that.

    "then you should use a reinforced product underneath and then skim with a regular body filler" - like ? Everglass or something ?
     
    missysdad1 likes this.
  7. NoelC
    Joined: Mar 21, 2018
    Posts: 667

    NoelC
    Member

    I say sarcastically, do what the professional do...or women all over the world. Layer it on, sculpt it till it smoothens out, color it up.
    As the song goes, she ain't pretty she just looks that way.
     

    Attached Files:

  8. 2OLD2FAST
    Joined: Feb 3, 2010
    Posts: 5,652

    2OLD2FAST
    Member
    from illinois

    Frightening !
     
    hidez57 and warbird1 like this.
  9. missysdad1
    Joined: Dec 9, 2008
    Posts: 3,307

    missysdad1
    Member

    In my humble opinion it's okay to use as much body filler as is necessary...as long as you get the metal clean, clean, clean before applying it. Wash with soap and water, then wipe thoroughly with a wax/grease remover...allowing it plenty of time to dry/evaporate before you shovel on the mud. Be sure to rough up the surface of the body filler before applying more on top of it.

    As has been mentioned, a reinforced filler such as MarGlass will seal any pinholes in your welds and provide extra strength to the panel if your filler is going to be thicker than 1/4" (my personal limit!) which it occasionally is in some cases.

    There are MANY TOP NAME BUILDERS who use A LOT of body filler in their builds. Use a premium brand (I prefer Rage Gold) and don't be afraid of it, most people will never know unless the panel gets damaged in use. Carry on!
     
    Last edited: Sep 5, 2022
  10. RmK57
    Joined: Dec 31, 2008
    Posts: 2,870

    RmK57
    Member

    I could that see that might make sense for ballast in the rear if your drag racing. I don't think I've ever seen filler laid on that thick before.
     
  11. Johnny Gee
    Joined: Dec 3, 2009
    Posts: 13,433

    Johnny Gee
    Member
    from Downey, Ca

    @NoelC based on your location. Bad Chad comes to mind.
     
  12. FAKKY
    Joined: Sep 9, 2016
    Posts: 295

    FAKKY
    Member

    Thanks all feeling less bad now.
    Yeah would think its 1/8-1/4" to fix most of the issues.

    The thicker parts (1/4" to 3/8"? ) would be where the panels dont align after fixing with patch - meaning I didnt get much of a curve in the patch to align with the rest of the truck so more straigh than curved. So might have to higher build there just to help contour and lign in ....... so to speak.
     
  13. FAKKY
    Joined: Sep 9, 2016
    Posts: 295

    FAKKY
    Member

    Just Gary likes this.
  14. We test these products rigorously. Yes there will always be tales of someone who got away with doing something not recommended but we don't make these recommendations up on a whim. Don't be the guy who listened to the "I've always done it this way and it was fine" users and has to redo it because it failed. I deal with those guys complaining about "product failures" all the time.
     
  15. FAKKY
    Joined: Sep 9, 2016
    Posts: 295

    FAKKY
    Member

    yeah there was a lot more bondo on this car than I realized ...... hence why cutting it all out to put metal there. BUt my fab work is not as good as I'd like it ...... so wasnt sure.
     
  16. angry
    Joined: Jan 6, 2006
    Posts: 344

    angry
    Member
    from ventura ca

    when it starts to lean it mite be to much
     
    XXL__, mrspeedyt, Tman and 1 other person like this.
  17. wheeldog57
    Joined: Dec 6, 2013
    Posts: 3,520

    wheeldog57
    Member

    @FAKKY in my own experience and limited bondo skills, I like to get the sheetmetal smooth enough that it needs 2 passes of bondo or less. And that is the hard part, sometimes I get to hack off my own repair and do it again!!
     
    INVISIBLEKID, Hutkikz and FAKKY like this.
  18. FAKKY
    Joined: Sep 9, 2016
    Posts: 295

    FAKKY
    Member

    lol
     
  19. Happydaze
    Joined: Aug 21, 2009
    Posts: 2,089

    Happydaze
    ALLIANCE MEMBER

    Always worth investing in your own metalworking skills. Op has made a promising start.

    Chris
     
    Driver50x and FAKKY like this.
  20. Hmmmm
    If you think about 1/4 of an inch of filler, thats a window that should be a minimum for body work. Doesn’t take a lot to get a panel within 1/4 inch of the correct contour.
    Location is important, 1/8 thick filler on a hood or roof could crack long before 1/4 in a door jamb ever would.
    Weld seams. I’ve melted out 1/2 of lead in some OE joints.
    If I had to go over that 1/4 inch threshold I think I’d look at a metal filler or kitty hair type product.
     
    wood remover, rod1 and SS327 like this.
  21. squirrel
    Joined: Sep 23, 2004
    Posts: 57,434

    squirrel
    ALLIANCE MEMBER

    Buiding an edge with thick filler....hmmm....not really the best idea. Try to get the metal to fit.
     
    Alaska Jim likes this.
  22. flamedabone
    Joined: Aug 3, 2001
    Posts: 5,571

    flamedabone
    ALLIANCE MEMBER

    On a slightly different note, are you overlapping your patch panels or butt welding? A proper butt welded panel will have both panels in the same plane without the ledge you are seeing.

    -Abone.
     
    alchemy and Hollywood-East like this.
  23. 51504bat
    Joined: May 22, 2010
    Posts: 5,153

    51504bat
    ALLIANCE MEMBER

    When I was in the Army I had a '63 4x4 carryall that a PO wrecked and had repaired in Mexico. The replacement passenger vent glass had Hecho in Mexico printed on it. Anyway the bondo around the lower right corner of the windshield was 1/2" to 3/4" thick. I'm guessing that's too much?
     
    mrspeedyt likes this.
  24. hemihotrod66
    Joined: May 5, 2019
    Posts: 968

    hemihotrod66
    Member

    I would do no more than a 1/4 inch of Bondo but lead is a whole different ballgame....
     
  25. 30dodge
    Joined: Jan 3, 2007
    Posts: 498

    30dodge
    Member
    from Pahrump nv

  26. Jalopy Joker
    Joined: Sep 3, 2006
    Posts: 32,274

    Jalopy Joker
    Member

    ^ yep, this still continues 20220905_155352.jpg
     
    2Blue2, 49ratfink and mrspeedyt like this.
  27. 41rodderz
    Joined: Sep 27, 2010
    Posts: 6,540

    41rodderz
    Member
    from Oregon

    You get better with practice, hopefully :D . Now is the time to practice. Learn from your mistakes and redo the metal work with more form and fitting.
     
  28. Squablow
    Joined: Apr 26, 2005
    Posts: 17,778

    Squablow
    Member

    I agree with FlamedAbone, looks like you might be overlapping your patch panels, which you really don't want to do. They should be butt welded to avoid that big ledge. Also, the entire seam needs to be welded, not tacked together like that first picture (I know you said that isn't yours, but that patch is very unfinished as it is pictured).

    An eighth to smooth it out is no problem if the underlying metal is clean. If you know it's going to be deeper than that (like a quarter), give a pass of kitty hair first, then knock that down until you can blend it all in with a skim coat of filler. If you know it's going to be 3/8" or more, try to work the metal more. Hammer and dolly, cut and re-weld, whatever you've got to do.

    It's hard (and often pointless) to get it perfect, but you don't want to do a total half-ass job either. Strive for those things and you'll be doing OK.
     
  29. stanlow69
    Joined: Feb 21, 2010
    Posts: 7,346

    stanlow69
    Member Emeritus

  30. PhilA
    Joined: Sep 6, 2018
    Posts: 2,075

    PhilA
    Member
    1. Hydro Tech

    ^ Where you cannot add passengers or gasoline, else you are in excess of the vehicle maximum gross weight before you even begin...

    I'm not averse to Bondo but only to fill the low points and smooth out imperfections. Troweled on with a garden shovel like that means you didn't do the metalwork right.
     

Share This Page

Register now to get rid of these ads!

Archive

Copyright © 1995-2021 The Jalopy Journal: Steal our stuff, we'll kick your teeth in. Terms of Service. Privacy Policy.

Atomic Industry
Forum software by XenForo™ ©2010-2014 XenForo Ltd.