    So I'm spraying single stage paint, after stripping panel down to metal, I applied summit voc 2k primer, sanded. Then summit voc black sealer, cleaned good then applied paint, the whole panel had fisheyes on it, so I drained compressor, I do have a small water separator at the compressor and at gun, so I got a piece of galvanized at home depot and cleaned it with wax and grease remover and prep sol, sprayed primer on it and looks like I have some very small bumps when zoomed in on camera. Any ideas what I should try next? 20220517_184105.jpg
     
  2. Derrick Boyle
    Joined: Jul 15, 2020
    Posts: 16

    Derrick Boyle

  3. 1time
    Joined: Dec 5, 2009
    Posts: 97

    1time
    Member
    from minnesota

    sand those little bumps with some 1000 grit paper and see what they are, possible solvent pocket, possible your material wasn't stirred or shaken properly, try filtering your material into your gun
     
    Just Gary likes this.

Share This Page

Register now to get rid of these ads!

Archive

Copyright © 1995-2021 The Jalopy Journal: Steal our stuff, we'll kick your teeth in. Terms of Service. Privacy Policy.

Atomic Industry
Forum software by XenForo™ ©2010-2014 XenForo Ltd.